WANG QING YANG ZHANG MU. A New Technique for Preparing the Fiber Preforms with Large Core and Large NA. [J]. (4):32-34(1988) DOI: 10.13756/j.gtxyj.1988.04.005.
A New Technique for Preparing the Fiber Preforms with Large Core and Large NA
摘要
本文介绍利用现有MCVD工艺制备大芯径、大数值孔径光纤预制棒的新工艺。在不掺硼的情况下
在预制棒芯层逐层减少SiCl
4
的流量
解决了为达到较高折射率差△n
在芯层掺锗过多
而引起光纤预制棒在沉积后期和缩棒过程中由材料的热膨胀系数而导致的炸裂问题。并通过改变火焰平移速度
提高了沉积速率
缩短了制棒时间。所拉制的光纤
数值孔径NA高达0.30。
Abstract
This paper presents the new technique for preparing the fiber preforms with large core and large N A by the conventional MCVD process. Under the condition of doping no Boron
Using the technique by decreasing the flow of SiCl
4
step by step in the core of the preforms
the problem of splitting caused by the different thermal expansion coefficient of the materials during the deposition and the depression as germanium is excessively doped in the core of the preforms for high refractive index defference An has been solved. By changing the moving velocity of the torch
the rate of deposition has been increased and the time for preparing the preforms has been shortened. The NA of the fibers to be drawn can be up to 0.30.